Home E-Mail Request Additional Information Polyester

 

SHINPEX - M TYPE

POLYESTER FILM

Thickness Range 12, 23, 36, 50 Microns (48, 92, 144, 200 Gauge )
Available width 400 mm--2200 mm (16--86 Inch )
Standard Length Per Roll 12 Mic. 12000, 18000, 24000, 36000, m
23 Mic. 6000, 9000, 12000, m
36 Mic. 4000, 8000,
50 Mic. 3000, 6000, m
Core I.D. 76.2 mm (3"), 152.4 mm (6")
Corona Treatment One Side Treatment
Application Metallising, Label, Decoration


Property

Unit

Test Method

TYPICAL VALUE

Thickness

Gauge

 

48+2.4

92+4.8

144+7.2

200+10.0

Microns

 

12+0.6

23+1.2

36+1.8

5+2.50

Conversion Yeild

m2/kg

 

59.7

31.14

19.9

14.33

in2/Ib

 

41970

21890

13990

10080

Tensil .........MD
Strength......TD

kg/mm2

ASTM-882

23+4

23+4

23+4

23+4

kg/mm2

ASTM-882

23+4

23+4

23+4

23+4

F-5 Value....MD

kg/mm2

ASTM-882

10

10

10

10

kg/mm2

ASTM-882

9

9

9

9

Elongation.....MD
At Break.......TD

%

ASTM-882

115+25

125+25

125+25

130+25

%

ASTM-882

115+25

125+25

125+25

130+25

Shrinkage.....MD
At 150
oC/30 min....TD

%

ASTM D-1204

1.5+0.5

1.5+0.5

1.5+0.5

1.5+0.5

%

ASTM D-1204

0+0.3

0+0.5

0+0.5

0+0.5

Friction Coefficent
Film to Film

s

ASTM D-1894

0.40+0.10

0.40+0.10

0.40+0.10

0.40+0.10

d

ASTM D-1894

0.40+0.10

0.40+0.10

0.40+0.10

0.40+0.10

Gloss

%

ASTM D-2457

130

150

150

150

Haze

%

ASTM D-1003

2.5+0.6

2.5+1.0

3.0+1.0

4.0+1.0

Moisture Vapor
Transmission Rate

g/100in2 24hr

ASTM E-96

2.75

1.48

-

-

g/m2 24hr

ASTM E-96

42

22

-

-

Oxygen
Transmission Rat
e

cm3/m2.24hr.atm25oCdry

9.78

5.74

-

-

cm3/m2.24hr.atm25oCdry

150

88

-

-

Wetting Index

dyne/cm3

54+4

54+4

54+4

54+4

Density

g/cm3

ASTM D-882

1.396

1.396

1.396

1.396

 